<?xml version='1.0' encoding='utf-8'?>
<?xml-stylesheet type="text/xsl" href="/v2/static/oai2.xsl"?>
<OAI-PMH xmlns="http://www.openarchives.org/OAI/2.0/" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/ http://www.openarchives.org/OAI/2.0/OAI-PMH.xsd">
  <responseDate>2026-09-18T22:03:21Z</responseDate>
  <request identifier="oai:figshare.com:article/30424960" metadataPrefix="oai_dc" verb="GetRecord">https://api.figshare.com/v2/oai</request>
  <GetRecord>
    <record>
      <header>
        <identifier>oai:figshare.com:article/30424960</identifier>
        <datestamp>2025-08-01T00:00:00Z</datestamp>
        <setSpec>portal_693</setSpec>
        <setSpec>item_type_8</setSpec>
        <setSpec>month_year_08_2025</setSpec>
      </header>
      <metadata>
        <oai_dc:dc xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance"  xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/" xmlns:dc="http://purl.org/dc/elements/1.1/" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/oai_dc/ http://www.openarchives.org/OAI/2.0/oai_dc.xsd">
          <dc:title>In Vitro Study Comparing Treatments for Incipient Enamel Lesion Remineralization</dc:title>
          <dc:creator>Aliyah Wilson (22481695)</dc:creator>
          <dc:subject>Pediatric Dentistry</dc:subject>
          <dc:description>Purpose: This study compared the remineralization efficacy of Icon™, 3M™ Varnish™ 5% Sodium Fluoride White Varnish (FV), and 38% Silver Diamine Fluoride (SDF; Advantage Arrest™) on enamel surfaces affected by incipient caries lesions.
Methods: Caries-free permanent teeth, extracted for orthodontic or surgical purposes, were obtained from the Pediatric Dentistry Department at UIC College of Dentistry. Enamel samples (4 mm x 5 mm) were prepared, frozen, and subjected to baseline microhardness testing. Samples were randomized into four groups (n=5/group): Icon, FV, SDF, and a control group. Artificial caries lesions were induced and treated per manufacturers’ instructions. Samples were immersed in a saliva-like remineralization solution for seven days, and post-treatment microhardness was assessed at 20 μm intervals to a depth of 200 μm. Statistical analyses included ANOVA with Tukey-Kramer post hoc tests and Generalized Estimating Equation (GEE) modeling.
Results: SDF demonstrated the lowest microhardness values, with a mean of 147.24 (SD: 39.76) at 100 μm, significantly lower than FV (276.54; SD: 33.72), Icon (254.59; SD: 30.18), and the control (253.19; SD: 36.16). FV and Icon showed significantly higher microhardness, indicating superior enamel strengthening compared to SDF. No significant differences were found between FV and Icon.
Conclusions: When managing incipient caries, all three materials are effective options for addressing early caries lesions. However, FV and Icon provided superior remineralization and surface hardening when compared to SDF.</dc:description>
          <dc:date>2025-08-01T00:00:00Z</dc:date>
          <dc:type>Text</dc:type>
          <dc:type>Thesis</dc:type>
          <dc:identifier>10.25417/uic.30424960.v1</dc:identifier>
          <dc:relation>https://figshare.com/articles/thesis/In_Vitro_Study_Comparing_Treatments_for_Incipient_Enamel_Lesion_Remineralization/30424960</dc:relation>
          <dc:rights>In Copyright</dc:rights>